Superalloy Centrifugal Impeller Vacuum Casting
Description
Basic Info.
Model NO. | Y30.1 |
Surface Roughness | Ra3.2 |
Machining Tolerance | +/-0.01mm |
Standard | ASTM |
High Temperature Duration | Above 40h |
Creep Tensile Strength at High Temperatu | Above 225MPa |
Test of Internal Defect | X-ray |
Test of Size | CMM |
Test of Surface Defect | Fpt |
Elongation of High Temperature | Above 3% |
Persistent Creep Temperature at High Tem | Above 975 Degree |
Tensile Strength of High Temperature | Above 830MPa |
Tensile Test Temperature | Above 900 Degree |
Transport Package | Plywood Boxes |
Specification | Diameter: 500mm |
Trademark | BoYuan casting |
Origin | Weifang City, Shandong Province, Shandong |
HS Code | 8414909090 |
Production Capacity | 100000pieces/Years |
Product Description
Product Description Superalloy turbine wheel used for turbojet engine, turbine wheel be finished by integral casting. And casting method of turbine wheel is investment & vacuum casting, casting surface smoothness can meet Ra3.2μm.
The material of turbine wheel is superalloy Inconel713c. And all turbine wheel are subjected to stress relief heat treatment to imporve the mechanical properties of products. After heat treatment mechanical properties can meet:
High temperature Tensile strength | ≥830MPa |
Elongation | ≥3% |
Persistent creep tensile strength at high temperature | ≥225MPa |
Persistent creep tensile strength of keeping time | ≥40H |
The blade thickness of turbine wheel is 0.4mm, the turbine roating speed is more than 60,000RPM.
What are the advantages of integral casting instead of welding process:
* The overall consistency of the turbine wheel is good
* The dynamic balance is good
* Production cost is lower
All turbine wheel will be done X-Ray inspection and fluorescent penetration test in our factory, including CMM, tensile strength test and hardness test.
Company Profile
Weifang Boyuan Power Technology Co., Ltd. specializes in the production of Aluminum Alloy impeller products and High temperature alloy impeller products,stainless steel impeller products. The company has a professional team that has long been engaged in the casting, processing and testing of impellers. Products are widely used in turbochargers, aero engines, industrial fans, compressors, blowers, rail transit, heavy mining machinery industry, refrigeration industry, marine engineering industry. The company has professional production line of Aluminum Alloy low pressure casting and high temperature alloy casting,stainless steel casting equipped with advanced inspection instrument. About casting production equipment we have: * Aluminum low pressure casting furnace * Vacuum casting furnace * Injection wax machine * Shell drying line * Constant temperature and humidity room * Plaster shell chamber * Sandblasting machine * Heat treatment furnace About machining equipment we have:
* DMG five axis machining center
* Three axis machining center
* Doosan CNC center Lathe
* General CNC Lathe
* Dynamic balancing machine
* Overspeed testing machine
* Radial Drilling machine
1. We can finish mould design and mould machining, mould assembly in our factory to ensure plan of casting
2. We can finish all casting and machining in our factory to ensure production time
3. We can finish all inspection in our factory to ensure production quality
Prev: ASTM GM13 Standard 0.5mm 0.75mm 1.0mm 1.5mm 2.0mm Smooth Textured HDPE Geomembrane Liner